Hello everyone,

We are using CI piping for fluid service containing NH3,CO2,H20 and H2S. The fluid composition is as follows:
NH3 = 0.402 kg/m3
CO2 = 0.255 kg/m3
H2O = 0.128 kg/m3
H2S = 0.0003 kg/m3
Temperature = 60-80Celcius
Pressure (psi) 14.7

The CI piping is suffering from thickness loss, pitting and pinholes. The corrosion of loss is not uniform and it is mostly localized. What could be the most possible material to shift too?

Thank you.

 
Replies continue below

Recommended for you

Do not double post on ENG-TIPS !!!!