Dear Community

I noticed that ASTM material for piping carbon steel (CS) and low temp carbon steel (LTCS)are similar in chemical composition and manufacturing process including heat-treatment. However, LTCS has a higher toughness for impact-test at -45 deg C (or -46 deg C).

I am referring to the following piping ASTM material :
Pipes : A106 Gr B vs A333
Forgings : A105N vs A350 LF2
Fittings : A234 vs A420

My query is which elements/factors cause the LTCS to have a higher toughness ?

I would pose a similar query on Pipeline, Piping & Fluid Mechanics Engineering Group.

regards

QWT
 
And don't make up new and useless acronyms.

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top