Sep 18, 2013 #1 albanbulku Mechanical Joined Mar 5, 2013 Messages 30 Location AL Which are the best electrodes to weld these grades of steel pipes ???? Pipe welding of S355j2(+ N) with api 5L x60 ?
Which are the best electrodes to weld these grades of steel pipes ???? Pipe welding of S355j2(+ N) with api 5L x60 ?
Sep 23, 2013 #2 stanweld Materials Joined May 9, 2003 Messages 2,906 Location US For the SMAW process, E7016/E7018 can be used. If full penetration from one side is required, E7010 should be used at least for the root and second pass. Upvote 0 Downvote
For the SMAW process, E7016/E7018 can be used. If full penetration from one side is required, E7010 should be used at least for the root and second pass.
Sep 24, 2013 Thread starter #3 albanbulku Mechanical Joined Mar 5, 2013 Messages 30 Location AL Thank you stanweld. How you think for E6010 for root pass) and E7018 for filler passes? Upvote 0 Downvote
Sep 24, 2013 #4 stanweld Materials Joined May 9, 2003 Messages 2,906 Location US Has been done many times. Upvote 0 Downvote
Sep 24, 2013 Thread starter #5 albanbulku Mechanical Joined Mar 5, 2013 Messages 30 Location AL So it is ok. Thanks for your answers mate. Upvote 0 Downvote