Which are the best electrodes to weld these grades of steel pipes ????

Pipe welding of S355j2(+ N) with api 5L x60 ?
 
Replies continue below

Recommended for you

For the SMAW process, E7016/E7018 can be used. If full penetration from one side is required, E7010 should be used at least for the root and second pass.

 
Thank you stanweld.

How you think for E6010 for root pass) and E7018 for filler passes?

 