Hi guys,
I am currently in a bind here.
Is there any ASME/ASTM code that specifies that body material of butterfly valve has to be the same as the pipe material?
So the service liquid is desalinated water, with TDS<10 ppm, pressure 7 bar, and T=40 deg C.
The pipe material that I have chosen is SS304L.
My butterfly valve's type is lug type, and currently I want to choose Ductile Iron as the body material, since butterfly valve's body is not the wetted part. There should be no issue with the water corroding the butterfly valve's body.
Since my butterfly valve is the lug type, I will connect the valve with the pipe by flange connection.
The flange material is also SS304L.
Will there be any corrosion issue if I choose ductile iron as the butterfly valve's body material?
Do any of you guys know the ASTM/ASME code that specify this issue?
While we are at it, I also want to ask, if I connect 2 flanges with different materials, for example, I connect SS flange with cast iron flange, with gasket in between, will there still be any corrosion issue?
Thanks guys for your help
I am currently in a bind here.
Is there any ASME/ASTM code that specifies that body material of butterfly valve has to be the same as the pipe material?
So the service liquid is desalinated water, with TDS<10 ppm, pressure 7 bar, and T=40 deg C.
The pipe material that I have chosen is SS304L.
My butterfly valve's type is lug type, and currently I want to choose Ductile Iron as the body material, since butterfly valve's body is not the wetted part. There should be no issue with the water corroding the butterfly valve's body.
Since my butterfly valve is the lug type, I will connect the valve with the pipe by flange connection.
The flange material is also SS304L.
Will there be any corrosion issue if I choose ductile iron as the butterfly valve's body material?
Do any of you guys know the ASTM/ASME code that specify this issue?
While we are at it, I also want to ask, if I connect 2 flanges with different materials, for example, I connect SS flange with cast iron flange, with gasket in between, will there still be any corrosion issue?
Thanks guys for your help