We are involved in designing a high temperature (500ºC) steam piping inside a power station. The pipe material selected is ASTM A335 P91 and the slippers (shoes/ saddles) of A387 Gr22.

Can somebody, having experience of designing piping for such temperature application recommend the correct/ proven type of slipper design?

Would it be ok to use standard welded design of slippers with the pipe? The concern is the differential thermal expansions between pipe and slipper - is a notch between either ends of the welded slipper design helpful?)

cheers,
 
Technical Note:
There is a posting previous of a slimmer problem and detail solution by

PREX
Advance Search (Heat Transfer & Thermodynamics engineering)

Reference Mechancial Design of Process System, by A. Keith Escoe. Gulf Publishing Company

I do not have my reference book with me on current assingment in Japan
 
Hello sbnz,

You should get a copy of Pipe Fabrication Institute (PFI) Bulletin ES-26. PFI ES-26 is referenced by ASME B31.1. This document addresses the manner and details of welding the support appurtenance to the pipe wall.

Regards, John.
 
I was thinking more in terms of a line tap
 