Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations Ron247 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Pipe Pile Fabrication Process

Status
Not open for further replies.

phamENG

Structural
Feb 6, 2015
7,729
This may not be the best place for this, but as "Off Shore Structure Engineering" is the only option in Marine/Ocean Engineering I'll give it a shot.

ASTM A252 Grade 3 Pipe piles for pier and marina construction. They are commonly available in ERW, roll and weld, and spiral weld. Is there any evidence (anecdotally or through rigorous research, though research is always better) of a variation in structural performance between the methods? I imagine the failure modes would vary some, but given the variables in marine structure design I tend to keep my designs conservative and well within the elastic range. Therefore, my question is primarily with regard to elastic behavior, though any insights would be appreciated.

Thanks!
 
Replies continue below

Recommended for you

I do find that the weld seam of carbon steel pipe corrodes at a substantially higher rate than the rest of the pipe. One type of construction may more detrimentally affected by this loss of the weld seam.
 