Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Pipe expansion help 1

Status
Not open for further replies.

tom73

Mining
Oct 9, 2006
3
I have 160 metres of 6" st/st metric pipe installed in a straight line,could anybody help me with the expansion rate of the pipe given the highest temperature it will see is 20 degC
 
Replies continue below

Recommended for you

150mm st/st 304 2mm wall....the max temp will be 25degc the min will be 15degc
 
Unrestrained expansion will be in the order of 27mm.

Mark Hutton


 
If you installed the pipe when it was 20 deg C then at 20 deg C it won't see any relative expansion. You need to take the temperature difference from ambient and not the absolute temperature to calculate expansion. The expansion could be anything.

corus
 
Have to agree with corus, if the pipe is installed at an ambient temperature of 20 degrees, the movement will become +/- 13mm. The change in length given in my previous post is for the whole 10degC range. The Engineering toolbox site is a useful design site, , with many design cooeficients and other useful information.