Hi,

I need some information regarding pinhole in HDPE gas pipe. I heard there is some information available in PPI.

Would anyone please let me know where I can find some pinhole information except ionixtechnologies info?

Thanks
Regards
Parvez
 
I suspect you may be referring to the paper, "Static control in PE Fuel Gas Pipe", that I think has been published in many forms over several years (with maybe latest at In any case I suspect GTI (formerly GRI etc.), as a result of their research/data gathering etc., likely knows something about this subject (if you have access to this resource/information).
 
(oops, I should have also mentioned "AGA")
 