WKTaylor
Well-known member
- Sep 24, 2001
- 4,174
WKTaylor (Aeronautics)
(OP)
31 Jul 19 19:41
Call-to-'ALL'...
Conventional resources do not provide insight into physical or mechanical properties for these alloys.
Original die Casting spec for these alloys is QQ-A-591 [similar to ASTM B85].
Cast parts are NOT Heat treated [F = 'as cast']
The base/procurement specs only list FTu & FTy... no other values for mechanical... and NO useful physical properties [IE: service temperatures, corrosion potential, conductivity, etc].
Anyone aware of source for definitive/authoritative physical/mechanical properties for these alloys?
Regards, Wil Taylor
o Trust - But Verify!
o We believe to be true what we prefer to be true. [Unknown]
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation,Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion", Homebuiltairplanes.com forum]