Civil/Environmental
Dec 16, 1999
6,868
I am trying to determine availability and cost to procure either 17-4PH or 15-5PH in 1.750 or 1.000 inch round or square bar stock. Is this material readily available in the US?
 
Replies continue below

Recommended for you

excellent reference
 
They are made by a number of US mills so sourcing through distribution should not be an issue.
Just remember that you will need to machine and heat treat it all, the cost of heat treating long pieces can be significant.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
You don't use these alloys in the annealed condition.
The annealed properties are very unreliable.

If there is any cutting, forming, or machining to do, then do it on the annealed material.
Then put them through the age hardening cycle.
If there is very little finish work (cut to length only) then you could age it all first.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 