Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

permissible number of times of flux reusing

Status
Not open for further replies.

leedrong

Mechanical
Joined
Aug 31, 2004
Messages
25
Location
KR
When welding of mild and high tensile carbon steel welding using AWS F76-EH14 rod and flux ( Submerge arc welding Process ) , What is the permissible number of times of flux reusing for welding quality control standpoint ?

We had an experiance that when we use mixed flux ,half new flux with half used flux which reused seberal times , we can see few spots on surface of bead and rarely observed cracks in deposited metal of thick plate welding .
 
leedrong;
First question - are you referring to "used flux" as slag OR flux that was not converted to slag during welding, but still looks like flux?

Second question - Do you have a closed loop recycling program for your SAW slag? What do you do with your slag from SAW?

Flux that has NOT reacted during the welding process (forming slag) can be picked up, and reused. From what I have read in AWS 5.17, there is no requirement limiting the number of times flux can be recycled with new (virgin) flux. However, it is important to note that contaminants like moisture, oil or debris can be picked up from the unused flux, thus contributing to your problem. I would not mix the unused flux with new flux. Unused flux could be captured and blended with crushed slag, and tested for electrode-flux reclassification in accordance with AWS guidelines.


The 1996 June edition of the AWS Welding Journal contains an excellent article on "Recycling of SAW Slag Proves Reliable and Repeatable".
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top