Hi all,
I´m facing the issue of trying to determine the permeability coefficient of -200mm rockfill!!?!? The gradation parameters are:
D100 = 200mm
D50 = 50mm
D10 = 7mm
This material is compacted with 16 metric tons vibratory compactors (6 passes). Does anybody have suggestions or knowledge of test being carried out on this coarse material.
Any comments would be appreciated.
cheers,
Throstur
I´m facing the issue of trying to determine the permeability coefficient of -200mm rockfill!!?!? The gradation parameters are:
D100 = 200mm
D50 = 50mm
D10 = 7mm
This material is compacted with 16 metric tons vibratory compactors (6 passes). Does anybody have suggestions or knowledge of test being carried out on this coarse material.
Any comments would be appreciated.
cheers,
Throstur