Does anyone have any reference for the performance of cast iron under fire load conditions?
 
Replies continue below

Recommended for you

Yes it cracks
lack of fibrous strength as in steel which melts, burns, distorts

crystal expansion
may stay for some time if the burn is off the pillar
but high heat is going to cause an expansion force at some junction at the very least