From
Our most advanced technology: we can make two different series of sintered NdFeB magnets--- ordinary book mold alloy and magnets (HAST NdFeB) based on a strip cast alloy which gives a better chemical stability. We has invested in the production technology enabling to use strip cast material. HAST NdFeB magnets have higher anticorrosion and can last for 7 days under 131 degree Celsius, 100% humidity and 3atm with loss of weight less than 5mg/cm2.
From
We produce ndfeb magnet without coating, many motor customers need passivated ndfeb magnet