I have a 1 1/2" thick lift lug that I am trying to analyze a 3/8" partial penetration weld all the way around the lug (see attached sketch).
Is there an effective throat calculation for partial pens like fillets (t=.707y)?
Thank you for your help.
Regards,
Is there an effective throat calculation for partial pens like fillets (t=.707y)?
Thank you for your help.