OK, break out "Structural Welding Code - Steel" AWS D1.1:200 for this question. Now go to p. 54, the figure at the bottom for double-bevel-groove weld. Look at the line for SMAW welding process. Everybody with me? I don't specify partial pens very often (maybe never) so I'm probably about to show my ignorance.
According to the chart T1 can be 5/16". The root face (f) has to be at least 1/8". This leaves 3/16" for S1 + S2. The total weld size (E1 + E2) = S1 + S2 - 1/4" which gives us negative 1/16" !!!
What am I not understanding here?
According to the chart T1 can be 5/16". The root face (f) has to be at least 1/8". This leaves 3/16" for S1 + S2. The total weld size (E1 + E2) = S1 + S2 - 1/4" which gives us negative 1/16" !!!
What am I not understanding here?