For welding a join with PJP, do we have qualication a WPS?

Thank you

 
Replies continue below

Recommended for you

Hi,

You can make use of a Pre-Qualified WPS as per Sec.3 of AWS D1.1 Code provided that your construction code is AWS D1.1 and the welding variables are with in the range specified in the code .
 
JATE,
As you have posted in the ASME section then yes, you do need a qualified WPS,