Hello All
I have a SS Pressure Vessel (Designed to Sec VIII Div 1). We have some stock SA 312/A 312 material (ERW pipe). To use this pipe in Pressure vessel as nozzle pipe (No objection by buyer for use of ERW pipes) is it required to have a partial data report.
What about welded fittings?
Do we need to have partial data report for Welded fittings
What are the circumstances (When procuring standard welded items) under which we require partial data report.
What about CS fittings or Pipes?
The reason for the above query is
A) Some of the SA material standards deals with Partial data report where as some other do not.
For example SA 312 does not discuss partial data report. SA 358 discusses about Partial data report.
In carbon steel case SA 234 WPB W does not discuss about partial data report
I have a SS Pressure Vessel (Designed to Sec VIII Div 1). We have some stock SA 312/A 312 material (ERW pipe). To use this pipe in Pressure vessel as nozzle pipe (No objection by buyer for use of ERW pipes) is it required to have a partial data report.
What about welded fittings?
Do we need to have partial data report for Welded fittings
What are the circumstances (When procuring standard welded items) under which we require partial data report.
What about CS fittings or Pipes?
The reason for the above query is
A) Some of the SA material standards deals with Partial data report where as some other do not.
For example SA 312 does not discuss partial data report. SA 358 discusses about Partial data report.
In carbon steel case SA 234 WPB W does not discuss about partial data report