Hi Gents,
We're facing very difficult situation for Aramco project as below.
Following is the requirement of SAES-H-002.
5.2.9 "The internal coating shall be extended up to the face of flat-and raised-face flanges that will not be in contact with the gasket. The coating applied shall be machined and ground to ensure that the surface is levelled properly and to avoid misalignment of gasket".
Status is as below.
1. Piping fluid is sea-water.
2. Internal surface of piping has been coated with FBE to prevent corrosion which will be caused by sea-water.
3. Flange surface is not coated.
4. Gasket does not cover up the whole surface of flange.
5. During commissioning, it has been found that the area (which is not covered with gasket) is corroded by sea-water.
Based on Aramco requirement aforementioned, client is requiring the area shall be coated or covered with new gasket.
Thus, we need the interpretation on Aramco requirement and to share your experiences in this case.
Thanks in advance
We're facing very difficult situation for Aramco project as below.
Following is the requirement of SAES-H-002.
5.2.9 "The internal coating shall be extended up to the face of flat-and raised-face flanges that will not be in contact with the gasket. The coating applied shall be machined and ground to ensure that the surface is levelled properly and to avoid misalignment of gasket".
Status is as below.
1. Piping fluid is sea-water.
2. Internal surface of piping has been coated with FBE to prevent corrosion which will be caused by sea-water.
3. Flange surface is not coated.
4. Gasket does not cover up the whole surface of flange.
5. During commissioning, it has been found that the area (which is not covered with gasket) is corroded by sea-water.
Based on Aramco requirement aforementioned, client is requiring the area shall be coated or covered with new gasket.
Thus, we need the interpretation on Aramco requirement and to share your experiences in this case.