Hi,

does someone know a paint system that will work on cast bronze? I need to paint some machined parts for sea water pumps which will be used in a marine environment. I don't know what the particular alloy is but most likely the parts contain lead.

any advice will be highly appreciated.
Thanks,,,

 
Replies continue below

Recommended for you

?

Are you not using a bronze that is resistant to seawater corrosion? If so, why paint it? If not, do you expect a coat of paint to make it resistant? If just for looks, I'd expect any decent epoxy paint to hold up well.
 