Hi everyone,
To build up a thickness of 600 um we are applying 3 coats of 200 um of the same paint material, I suppose it's to avoid sagging during application but when on the first coat we achieve a thickness over the spec the client ask to sand down. I'm wondering if we achieve 600 um with a single coat if the integrity of the paint would be any different than with 3 coats, would we get cohesion failure on a pull-off test?
To build up a thickness of 600 um we are applying 3 coats of 200 um of the same paint material, I suppose it's to avoid sagging during application but when on the first coat we achieve a thickness over the spec the client ask to sand down. I'm wondering if we achieve 600 um with a single coat if the integrity of the paint would be any different than with 3 coats, would we get cohesion failure on a pull-off test?