what is the best type of paint for use outside in an area close to the coast?
 
Replies continue below

Recommended for you

Best coating--hot dipped galvanizing

Next best--inorganic zinc over white metal
 
You asked the $64,000,000 question. I have to evaluate coating proposed for US Navy equipment all the time and I found this table a few years ago that I just love. It rates paint coatings on steel based on the surface preparation, environment and service life. I use it to specify performance with statements like: "Coatings shall have a minimum expected life of 15 years in a Seacoast Marine Heavy Industrial envioronment when rated per NACE paper No. 477 or similar nationally recognized rating system". This reference is a more concise table printed by a paint manufacturer. I have printed out the actual report but I couldn't find the web reference right off. It is from the 1996 Inernational Corrosion Conference.

 
Interesting table, RockEngineer. Intriguing that no ratings are shown for galvanising, either as a stand alone coat or as the first of a system. Since it was produced by a paint manufacturer, I guess that explains it.
 