Hi all,

Observation: Paint flaking/getting peeled off easily( white metal is visible now)
Equipment: Piping(HDG)+ epoxy mastic coating( 3 coats)

We want to repair these peeled off areas. Is there any standards which describes how much area to be removed(Surface preparation) for the repair these damages?
 
Replies continue below

Recommended for you

I don't know if this is an issue, but with HDG, you have to be careful of the coating system. Zinc saponification can occur and lead to a coating failure.

So strange to see the singularity approaching while the entire planet is rapidly turning into a hellscape. -John Coates

-Dik
 