Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Paint pigments

Status
Not open for further replies.

kiddhill20

Mechanical
Joined
Jan 29, 2004
Messages
6
Location
CA
Hello all,

I heard from someone that there are paint pigments that are currently encapsulated in silicon (for what reason I'm not sure) but I haven't been able to find any information concerning this.

Can anyone suggest a good place to start? Thanks very much.
 
Perhaps he meant silicone or was refering to silane surface treatments. Silicon make no sense in this context.
 
Thanks for the reply, Compositepro. I found it's silica. Pigment manufacturers use a slurry of the pigment together with a sodium silicate solution at a particular pH to coat the pigments. (Process has actually been around since the 1970s... just looked in the wrong places...)

I have read that it is the hydrophilicity of the pigment surface that enables silica to deposit and form a coating. Does anyone know of another reason that I may not be aware of?
 
Sodium silicate is also know as water glass. I believe its main function is as a high temperature binder. So those pigments are probably used for high temperature paints.
 