Where can I find a paint product that can be applied to glass that will give an etched or frosted look?
 
It will probably be some sort of acid or silk screening process, not really a paint.

[green]"Art without engineering is dreaming; Engineering without art is calculating."[/green]
Steven K. Roberts, Technomad
Have you read faq731-376 to make the best use of Eng-Tips Forums?
 
Hydrofluoric acid (HF) is used to etch glass.
It's sometimes used as an ingredient in cleaners for aluminum wheels -- check the ingredients on some aerosol cans in your local auto parts store.
 
Search this forum for "glass paint", the subject has come up before, and IIRC, one of the mentioned suppliers had a paint/glaze product that would produce frosted and/or crackled finishes.
 
I found a manufacture of waterbased paint for glass. They have many different finishes. Conatct them if you require the product. Strata Paint. 450-662-2537
 
Correction the number for Strata is 514-910-1134
 