Today we had to use an alternative to toughened PA66 as there appears to be a shortage of the stuff.
We used a toughened PA6. The finish was awful - dull/patchy etc. (Yes, it was dry, melt temperature as measured was in middle of range, blah blah, etc.)
In came my sales manager and suggested adding 2% masterbatch with a PE carrier. Never heard of this before but gave it a go - lo and behold a dramatic improvement in SF!
Any facts or theories why this should be?