waross
Electrical
- Jan 7, 2006
- 28,237
Gotta throw the BS flag on that statement.bridgebuster's linked said:It is clear that the fractured member was carrying no load
How to explain the 2 inch plus displacement when the ability to carry the non-existent load was lost.
Bill
--------------------
"Why not the best?"
Jimmy Carter