I would like to weld P8 TO P10
Can i used p8 to p8 OR P10 TO P10 PQR TO MAKE P8 TO P10 WPS.
Please advice
stan
 
Replies continue below

Recommended for you

AS I understand as per QW-424.1
i cannot used P8 TO P8 OR P10H TO P10H ( PQR) TO MAKE NEW WELD PROCEDURE FOR P8 TO P10
OR
can not used P8 TO P8 OR P10H TO P10H WELDING PROCEDURE TO WELD P8 TO P10H

Please confirm

 
Does your company not want to pay for someone with appropriate qualifications or experience to answer these questions ?
Or are they happy for you to continually ask for advice on an internet forum ?
Or, are they paying you for your knowledge and experience and yet you are getting all your answers from internet forums ?
 
You need to qualify a P8 to P10 procedure per Section IX.
 
DekDee said:
Does your company not want to pay for someone with appropriate qualifications or experience to answer these questions ?
Welding engineering is the most heavily poaching specialization in the engineering profession, by other engineers and by non-engineers. Here in Ontario, to qualify to submit a PQR for registration with the TSSA, all you require is a method of payment.
The unasked (and scary) question in this thread is how P10 will be welded to P10...