Hello All,
Code is ASME B31.1 2014.
Issue is a 32" P22 Sch60 pipe weld just below flush that had water inadvertently released and 'quenched' the weld enough to cause the heat treat chart to drop below the WPS inter-pass temp. The temp. dropped from 500F to 250F briefly. 400F-600F is WPS inter-pass range. In cases where chrome pipes were quenched during PWHT, replacing all affected pipes was the course of action.
The code will not address this directly. This is an NCR at best but is it necessary to replace the pipe and 90 elbow? Hydrogen bake out was performed and pending RT. Safety and quality are the top concerns but schedule and commercial are also considerations. That is, we will replace if necessary but no contractor wants to replace unless absolutely necessary. That is a huge expense. I do not represent the contractor.
Seeking advice on options on the path forward. We have a chart that shows a temp. drop. You can't ignore that. Replacement is worst case scenario. Is a partial machine/grind/reweld of 50% reasonable? Complete cut out and re-weld of the same material, no replacement? Boat Sample? Hardness test? Brittlement, ductility and grain structure are concerns but how to determine if the weld/pipe was 'actually' damaged.
Thanks for any advi
Code is ASME B31.1 2014.
Issue is a 32" P22 Sch60 pipe weld just below flush that had water inadvertently released and 'quenched' the weld enough to cause the heat treat chart to drop below the WPS inter-pass temp. The temp. dropped from 500F to 250F briefly. 400F-600F is WPS inter-pass range. In cases where chrome pipes were quenched during PWHT, replacing all affected pipes was the course of action.
The code will not address this directly. This is an NCR at best but is it necessary to replace the pipe and 90 elbow? Hydrogen bake out was performed and pending RT. Safety and quality are the top concerns but schedule and commercial are also considerations. That is, we will replace if necessary but no contractor wants to replace unless absolutely necessary. That is a huge expense. I do not represent the contractor.
Seeking advice on options on the path forward. We have a chart that shows a temp. drop. You can't ignore that. Replacement is worst case scenario. Is a partial machine/grind/reweld of 50% reasonable? Complete cut out and re-weld of the same material, no replacement? Boat Sample? Hardness test? Brittlement, ductility and grain structure are concerns but how to determine if the weld/pipe was 'actually' damaged.
Thanks for any advi