Aug 13, 2002 #1 Ryno Mechanical Joined Aug 13, 2002 Messages 2 Location US I need to find a reference for P-numbers: specifically I need to learn about P-1, P-2,P-4, P-5A, P-5B, P-8, P91
I need to find a reference for P-numbers: specifically I need to learn about P-1, P-2,P-4, P-5A, P-5B, P-8, P91
Aug 20, 2002 1 #2 apiguy Mechanical Joined Mar 5, 2002 Messages 116 Location US ASME Section II Part D should provide some insight as to which ASTM/ASME spec number s to deal with and which materials fall into which groups. Then procede to either the ASTM or ASME section mfor the spec. number The APIGUY.... Upvote 0 Downvote
ASME Section II Part D should provide some insight as to which ASTM/ASME spec number s to deal with and which materials fall into which groups. Then procede to either the ASTM or ASME section mfor the spec. number The APIGUY....