Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

P NUMBER FOR TOOL STEEL W1 2

Status
Not open for further replies.

andyweld

Nuclear
Mar 21, 2008
18
Does anybody know the P NUMBER (or S number) FOR TOOL STEEL W1 for procedure qualification?

Thanks
 
Replies continue below

Recommended for you

Thanks for the link.
Checked, doesn't seem it is on it.

 
well tool steel is really not real weldable, least I wouldn't try it.

I guess some folks are set up for it
 
andyweld;
There is no P-No for this steel. Why do you need one? Just list the base material designation as W1 Tool Steel on the WPS.
 
Thanks for the reply. One more question, normally what filler material is used for TIG welding this material?
 
andyweld;
This tool steel is a high carbon low alloy steel that can be welded with local preheat only (300 deg F). I would use a carbon steel filler metal or Inconel (Inco A) depending on the function of the weld.
 