Oversized tap for internal threads mating with HDG bolt

Status
Not open for further replies.

boltengineer

Mechanical
Dec 21, 2007
1
Does anyone know of a tool manufacturer that will make special taps? I need an oversized tap that will meet the allowable dimensions in ASTM A563 for overtapping nut thread to permit assembly on a hot dipped galvanized bolt. I am having no luck getting anyone I know of to make this.
 
Replies continue below

Recommended for you

I have worked with MSC tool company directly here in the US when looking for oversize taps. Although they don't manufacture anything, they were able to order a custom tap through a "confidential supplier".

-Reidh

 