What will be overtolerance on thickness of 3mm thick sheets of ASTM A537 and ASTM A516?
Regards,
Ijaz
 
Replies continue below

Recommended for you

Both materials are manufactured to A20, thus A20 Table A2.1 lists the over and under thickness tolerances.

The table only goes down to 5.0 mm, but per Note 3 you would use the 5.0 mm tolerances.
 