Hi,
I have a two layered skin panel. One layer is 0.200” inch thick and the other layer is 0.050” thick.
BACR15FV8KE(*) rivet will be installed in this panel. Head will be on the thicker panel side and tail on the 0.050” thick panel.
Is there is a minimum skin thickness requirement regarding overdriving of the FV rivet? Can the buck tail be over driven to 1.5D or this will damage the 0.050” thickness panel in the process?
Thanking everyone in advance for their response.
I have a two layered skin panel. One layer is 0.200” inch thick and the other layer is 0.050” thick.
BACR15FV8KE(*) rivet will be installed in this panel. Head will be on the thicker panel side and tail on the 0.050” thick panel.
Is there is a minimum skin thickness requirement regarding overdriving of the FV rivet? Can the buck tail be over driven to 1.5D or this will damage the 0.050” thickness panel in the process?