Hi
looking for a place to get compresive strenghs of materials. I looked at matweb.com but they do not have comprsive strengths, unless it is called something else. Can anyone lead me in the right direction.
thanks
greif
 
Replies continue below

Recommended for you

What are you trying to do? If you're trying to calculate if a colum will buckle you will need Euler's slenderness ratio, Modulus of Elasticity, and Moment of Inertia.

Best Regards,

Heckler
Sr. Mechanical Engineer
SW2005 SP 5.0 & Pro/E 2001
Dell Precision 370
P4 3.6 GHz, 1GB RAM
XP Pro SP2.0
NVIDIA Quadro FX 1400
o
_`\(,_
(_)/ (_)

Never argue with an idiot. They'll bring you down to their level and beat you with experience every time.
 
If you have access to Roark's formulas for stress and strain check chapter 14. This chapter goes into great detail on elastic stability of compression members

Best Regards,

Heckler
Sr. Mechanical Engineer
SW2005 SP 5.0 & Pro/E 2001
Dell Precision 370
P4 3.6 GHz, 1GB RAM
XP Pro SP2.0
NVIDIA Quadro FX 1400
o
_`\(,_
(_)/ (_)

Never argue with an idiot. They'll bring you down to their level and beat you with experience every time.
 