I have a situation where a barren organic tank is vented and the contaminants in the airstream include kerosene, amine, and isodecanyl.
I was thinking about using a fiberglass style of duct for this particular scenario as the tanks are made of fiberglass but was wondering if anyone else has seen a different material used in industry?
The organic compounds are reacting with the CPVC piping causing brittle fracture.