What is the optimum root opening, for complete penetration weld, in a single pass, one side only for the material and joint described below?
Weld process is GTAW, 3/32 tungsten, 2% thor.
Titanium 6Al 4V, 0.100” thick
Single V butt joint, 60 Deg included angle with 0.025 root face.
Also, please direct me to any formulas that apply for determining root opening.
Thank you,
Dave
Weld process is GTAW, 3/32 tungsten, 2% thor.
Titanium 6Al 4V, 0.100” thick
Single V butt joint, 60 Deg included angle with 0.025 root face.
Also, please direct me to any formulas that apply for determining root opening.
Thank you,
Dave