Hi All,
We are working with a Viton GF600S material and require the best finish possible. Does anyone have any experience as to what the minimum mold finish should be (e.g. 8uIN, etc.) for the part to have the smoothest texture possible? Part thickness is .050" x .69 dia.
Also, is there a point of "dimishing returns" where going finer in finish does not produce any smoother texture on the molded part? We are considering either chroming, Aluminizing, TiN or NiCo Tef coatings to aid in release. Anyone have experience or a preference?
Thanks,
Glenn
We are working with a Viton GF600S material and require the best finish possible. Does anyone have any experience as to what the minimum mold finish should be (e.g. 8uIN, etc.) for the part to have the smoothest texture possible? Part thickness is .050" x .69 dia.
Also, is there a point of "dimishing returns" where going finer in finish does not produce any smoother texture on the molded part? We are considering either chroming, Aluminizing, TiN or NiCo Tef coatings to aid in release. Anyone have experience or a preference?
Thanks,
Glenn