Folks

We need to apply a static 1000lbs tensile load to a step bar but my concern is necking rupture. Material is Steel 4130. Is there a formula to estimate the optimum fillet radius to use? or whether a draft taper will work better? If not, a FEA software like Creo structure will work as well??

neck_yfsh0i.png
 
pyromech,

I would have thought the the best fillet radius is the biggest one possible.

--
JHG
 
Optimum for what?

Lowest stress? Lowest cost? Lowest weight? Least material removed? Most difficult to machine?
 
swertel said:
Get a copy of Peterson's Stress Concentration Factors.
Thanks. there might not be a formula for two parts with different cross sections.
 
Only 1000 lbs? What are required minimum dims of the dia (upper) and rect (lower) sections?
What's the cyclical rate of loading?
 
Call the machine shop and ask how they would machine the fillet and what radii are convenient. Round up from any calculation to one of these.
 