Folks
We need to apply a static 1000lbs tensile load to a step bar but my concern is necking rupture. Material is Steel 4130. Is there a formula to estimate the optimum fillet radius to use? or whether a draft taper will work better? If not, a FEA software like Creo structure will work as well??