What are others experience on improvement of refinery Claus units reliability, on the aspects concerning acid gas and SWS gas feeds quality, plugging, corrosion, concrete damages, main burner NH3 destruction, insulation and steam tracers. Because of environment protection I suppose that a discussion on this subject should be useful for all of us.