GregLocock
Automotive
They used Reinforced Autoclaved Aerated Concrete to build large parts of the roof. Water ingress damages RAAC. Water is often present on roofs.
Odd how this huge problem comes up just as they want to repurpose the site.
Here's the technical reports
The Building C report describes RAAC in some detail.
Cheers
Greg Locock
New here? Try reading these, they might help FAQ731-376
Odd how this huge problem comes up just as they want to repurpose the site.
Here's the technical reports
The Building C report describes RAAC in some detail.
Cheers
Greg Locock
New here? Try reading these, they might help FAQ731-376