Has anyone come against a problem called onion skin, aka kish? This problem is a formation of a difficult to pickle scale on primary steel.

Let me know if anyone has heard or solved this problem.
 
Replies continue below

Recommended for you

Grades - high carbon (0.50 and higher); 4130; 10B38

Hot Process - CSP caster into a 7 stand rolling mill. Approximatley 1600 finishing temp and 1190 coiling.

No processing prior to pickling; no scale breaker at pickle line either.
 