I want to develop a heat treatment station to treat aisi 1070 1 mm thick about 160 to 280 mm diameter.
It will be under atmosphere controlled using mixture of a inert gas plus methane or propane to have the same Carbon potential.
This material comes from a laser cutting vendor , cold rolled , with 102 HRB [HRC 25.6 ]
It shall be harden to HR 45N : 67 min [ HRC 61] at 850 °C
The quenching will be with oil at 100°C or other if better.
Then temper under inert atmosphere in a fixture that will press it so it get flatten, with a harden of HRA 70 71 [ HRC 39 14 ] as resultant
The temper will be at 520°C for 4 hours
The chamber shall be about 300 x 300 x 300 mm
Because the rise of the u$s from 1 to 3,80 in the last 3 months, in my country , it is impossible to buy from any vendor, and furthermore, I take it as a challenge.
I thought in some thing like a top loading, with internal oil under the same atmosphere, but it shall be temporally closed while heating, this is the not know by me how to do this device .
The scope is to have the piece with the same surface when coming from the vendor, a brigth clean surface.
The piece will be cleaned after quenching and the tempered in the same chamber but with a pure inert gas , could be N2 or , Ar,
The production rate is from 1 to 20 pieces . We can say at lab rate.
Pardal