haynewp
Structural
- Dec 13, 2000
- 2,329
I am doing the analysis on roof bowstring trusses from 1943. The attached note I think means the wood was to have 900 psi bending strength and 1200 psi axial but I am not sure. It looks like there may be an "f" after the 1200 psi. The tensile strength of wood is commonly listed as much lower than the parallel to grain compressive strength in NDS. If the 1200 psi represents axial, was it common back then to use that for both tension and compression?