I have an old engineering drawing that refers to Uranus R1. Can anyone identify this or point me in the right direction? I understand that the Uranus brand name was used by Creusot Loire Industries in France but the company folded in 1984.
 
Replies continue below

Recommended for you

well more like it was absorbed or merged. The Uranus trade names are still used. That said I don't remember R1.
If no one else answers I'll check tomorrow when I am in the office.

= = = = = = = = = = = = = = = = = = = =
Still trying to help you stop corrosion.
formerly Trent Tube, now Plymouth Tube
eblessman@plymouth.com
or edstainless@earthlink.net
 
I checked Woldman's 5th edition and could not find an R1 designation, only an F1 from a Hidalgo Steel in New York.

Maybe a more recent Woldman's includes an R1.
 
My Woldman's only lists Uranus R3 which is now listed as ZCR157, which is a 15% Cr, 7% Ni, 2.2% Mo precipitation hardening stainless steel.

 