vahabsolgi
Mechanical
Hi every body
I want to seal an electrode which is installed into a hole with an viton material O-ring. The o-ring size is 3mm as inner diameter and 1.5mm as thickness. The operation pressure is 30bar and the maximum temperature will be 120 degree centigrade. the o-ring is 0.6mm compressed after installation. Other dimensions have been mentioned in the attached link.
After assembling this setup it is noticed that there is a leakage even in lower pressures (10 bar) in the place of sealing o-ring.
I would like to help me and tell me where is the mistake and how should I change the design to overcome this problem.
Moreover is there a standard maximum pressure range which small o-rings can seal?
I want to seal an electrode which is installed into a hole with an viton material O-ring. The o-ring size is 3mm as inner diameter and 1.5mm as thickness. The operation pressure is 30bar and the maximum temperature will be 120 degree centigrade. the o-ring is 0.6mm compressed after installation. Other dimensions have been mentioned in the attached link.
After assembling this setup it is noticed that there is a leakage even in lower pressures (10 bar) in the place of sealing o-ring.
I would like to help me and tell me where is the mistake and how should I change the design to overcome this problem.
Moreover is there a standard maximum pressure range which small o-rings can seal?