kilrbee

Chemical
Sep 2, 2006
41
I am taking a Zytel part, and modifying it for prototyping. It will involve build up and maching of part of the piece, similar to using fiberglass and resin. I need something that will bond to the nylon.

Can I get some ideas on what materials/process to use?

Michael
 
Replies continue below

Recommended for you

Concentrated Formic acid is still the best adhesive I know for solvent welding nylon.

It has very iritating fumes and burns the skin, so gloves, safety glasses fume extraction etc are advised.

To give it more body to build a fillet, you can dissolve some resin shavings in the acid to make a full bodied adhesive.

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor