Hi All,
I'm working on a project that requires an NSF-61 certified cement lining or coating. Application to meet AWWA C205 standards as well.
Any one know of any products on the market that meet this criteria?
Thanks,
 
Replies continue below

Recommended for you

Thanks rconner,
I looked into however this NSF certification is site-specific for their pipe and fittings as a whole product, fabricated and cement-lined in their shop. The actual cement material is not available on the market as an NSF-61 product.
I've found others similar.

Another issue is finding a cement mortar lining material that complies with both ANSI/AWWA and NSF-61. I can only find one so far. Apparently it's difficult to locate uncontaminated raw materials.
thanks
 